SABIC® HDPE B4660

Want to keep this datasheet? Save it now in your required format

Description

B4660 grade are medium molecular weight High Density Polyethylene homopolymer for blow molding Applications. They are primarily Designed for imparting high rigidity, toughness and good processability. These unique properties offer the possibility to reduce weight at very good top load strength. B4660: Suitable for Dairy products and Juice Packaging

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Material materials with Density of 0.96 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

500 %

Show Material materials with Elongation of 500 %

ASTM D638

Flexural modulus

23.0 °C

1.1 GPa

Show Material materials with Flexural modulus of 1.1 GPa

ISO 178/1A

Flexural strength

23.0 °C

28 MPa

Show Material materials with Flexural strength of 28 MPa

ASTM D790

Hardness, Shore D

23.0 °C

66 [-]

Show Material materials with Hardness, Shore D of 66 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

150 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 150 J/m

ASTM D256

Tensile strength

23.0 °C

18 MPa

Show Material materials with Tensile strength of 18 MPa

ASTM D638

Yield strength

23.0 °C

30 MPa

Show Material materials with Yield strength of 30 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

127 °C

Show Material materials with Vicat softening temperature of 127 °C

ASTM D1525

Rheological Properties

PropertyValueComment

Melt mass-flow rate

0.7 g/10min

Show Material materials with Melt mass-flow rate of 0.7 g/10min

ASTM D1238 | 190°C/2.16 kg

Technological properties

Property
Application areas

Dairy products, Juice Packaging