SABIC® HDPE B5206

Want to keep this datasheet? Save it now in your required format

Description

HDPE B5206 is high density polyethylene specially developed for large blow molding / Jerry cans. The material offers high stiffness, good processability and excellent combination of stiffness/ESCR.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.05 GPa

Show Material materials with Elastic modulus of 1.05 GPa

ASTM D638

Elongation at yield

23.0 °C

10 %

Show Material materials with Elongation at yield of 10 %

ISO 527-1/-2

Impact strength, Charpy notched

-30.0 °C

36 kJ/m²

Show Material materials with Impact strength, Charpy notched of 36 kJ/m²

ISO 179

Yield strength

23.0 °C

26 MPa

Show Material materials with Yield strength of 26 MPa

ASTM D638

Rheological Properties

PropertyValueComment

Melt mass-flow rate

6.5 g/10min

Show Material materials with Melt mass-flow rate of 6.5 g/10min

ISO 1133 | 190°C/21.6 kg

Technological properties

Property
Application areas

Jerry cans