SABIC® HDPE B5429

Want to keep this datasheet? Save it now in your required format

Description

B5429 grade is medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades offer excellent combination of toughness, stress cracking resistance, load bearing strength with easy processability. The grade available with antistatic additive is B5429A.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1 GPa

Show Material materials with Flexural modulus of 1 GPa

ISO 178/1A

Flexural strength

23.0 °C

25 MPa

Show Material materials with Flexural strength of 25 MPa

ASTM D790

Hardness, Shore D

23.0 °C

65 [-]

Show Material materials with Hardness, Shore D of 65 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

180 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 180 J/m

ASTM D256

Tensile strength

23.0 °C

19 MPa

Show Material materials with Tensile strength of 19 MPa

ASTM D638

Yield strength

23.0 °C

28 MPa

Show Material materials with Yield strength of 28 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

124 °C

Show Material materials with Vicat softening temperature of 124 °C

ASTM D1525

Technological properties

Property
Application areas

Bottles & cans,Containers & pails