Automotive. Low gloss, color concentratable for interior applications. Natural only.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.05 g/cm³

Show Material materials with Density of 1.05 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.2 GPa

Show Material materials with Elastic modulus of 2.2 GPa

ASTM D 638 | 5 mm/min

Flexural modulus

23.0 °C

2.41 GPa

Show Material materials with Flexural modulus of 2.41 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural yield strength

23.0 °C

72 MPa

Show Material materials with Flexural yield strength of 72 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Impact strength, Izod notched, ASTM

23.0 °C

186 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 186 J/m

ASTM D 256

Yield strength

23.0 °C

48 MPa

Show Material materials with Yield strength of 48 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.55E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.55E-4 1/K

ASTM E 831 | -40°C to 60°C

Heat deflection temperature, 1.80 MPa

85 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed

Relative temperature index, electrical

60 °C

Show Material materials with Relative temperature index, electrical of 60 °C

UL 746B

Relative temperature index, mechanical impact

60 °C

Show Material materials with Relative temperature index, mechanical impact of 60 °C

UL 746B

Relative temperature index, mechanical strength

60 °C

Show Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746B

Flammability

UL Recognized, 94HB Flame Class Rating | 1.47mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

1 V

Show Material materials with Comparative tracking index of 1 V

UL 746A

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

3.3 g/10min

Show Material materials with Melt mass-flow rate of 3.3 g/10min

ASTM D 1238 | 230°C/3.8 kg

Melt viscosity

23.0 °C

155 Pa·s

Show Material materials with Melt viscosity of 155 Pa·s

ASTM D 3825 | 260°C, 1000 sec⁻¹

Shrinkage

23.0 °C

0.5 - 0.8 %

Show Material materials with Shrinkage of 0.5 - 0.8 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Auto Aftermarket,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Recreational Vehicle

Processing methods

Drying Temperature: 90-95°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.1%, Melt Temperature: 230-275°C, Nozzle Temperature: 230-275°C, Front - Zone 3 Temperature: 220-255°C, Middle - Zone 2 Temperature: 210-250°C, Rear - Zone 1 Temperature: 195-240°C, Mold Temperature: 50-80°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm