SABIC® LLDPE C2820T

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE C2820T is a butene linear low density polyethylene resin typically designed for easy processing and specially formulated for optimum thermal stability at high temperatures used in casting film extrusion. Cast film product from SABIC® LLDPE C2820T exhibit excellent optical properties, easy processing & energy saving, excellent thickness uniformity, improved machine output, well controlled die line. SABIC® LLDPE C2820T is TNPP free grade. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Optical

PropertyValueComment

Haze

7 %

Show Material materials with Haze of 7 %

ASTM D1003

Rheological Properties

PropertyValueComment

Melt mass-flow rate

2.8 g/10min

Show Material materials with Melt mass-flow rate of 2.8 g/10min

ASTM D1238 | 190°C/2.16 kg

Technological properties

Property
Application areas

Blown film