SABIC® HDPE CC453

Want to keep this datasheet? Save it now in your required format

Description

SABIC HDPE CC453 is a High Density Polyethylene specially developed for the injection and compression molding of caps & closures for the packaging of beverages. This grade offers an ideal combination of impact strength, ESCR and meet organoleptic properties requirements.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

0.8 GPa

Show Material materials with Flexural modulus of 0.8 GPa

ISO 178/1A

Flexural strength

23.0 °C

21 MPa

Show Material materials with Flexural strength of 21 MPa

ASTM D790

Hardness, Shore D

23.0 °C

60 [-]

Show Material materials with Hardness, Shore D of 60 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

150 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 150 J/m

ASTM D256

Tensile strength

23.0 °C

21 MPa

Show Material materials with Tensile strength of 21 MPa

ASTM D638

Yield strength

23.0 °C

23 MPa

Show Material materials with Yield strength of 23 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

125 °C

Show Material materials with Vicat softening temperature of 125 °C

ASTM D1525

Technological properties

Property
Application areas

Bottles,Multi purpose injection moulding