CYCOLAC™ Resin EX39F

Want to keep this datasheet? Save it now in your required format

Description

Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.03 g/cm³

Show Material materials with Density of 1.03 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.68 GPa

Show Material materials with Elastic modulus of 1.68 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

108 %

Show Material materials with Elongation of 108 %

ASTM D 638 | Type I, 5 mm/min

Elongation at yield

23.0 °C

3.5 %

Show Material materials with Elongation at yield of 3.5 %

ASTM D 638 | Type I, 5 mm/min

Flexural modulus

23.0 °C

1.9 GPa

Show Material materials with Flexural modulus of 1.9 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural yield strength

23.0 °C

57 MPa

Show Material materials with Flexural yield strength of 57 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Impact strength, Izod notched, ASTM

-30.0 °C

320 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 320 J/m

ASTM D 256

23.0 °C

464 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 464 J/m

ASTM D 256

Tensile strength

23.0 °C

28 MPa

Show Material materials with Tensile strength of 28 MPa

ASTM D 638 | Type I, 5 mm/min

Yield strength

23.0 °C

35 MPa

Show Material materials with Yield strength of 35 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.01E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.01E-4 1/K

ASTM E 831 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

1.17E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.17E-4 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

77 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 77 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Melting point

210 - 225 °C

Show Material materials with Melting point of 210 - 225 °C

Relative temperature index, electrical

60 °C

Show Material materials with Relative temperature index, electrical of 60 °C

UL 746B

Relative temperature index, mechanical impact

60 °C

Show Material materials with Relative temperature index, mechanical impact of 60 °C

UL 746B

Relative temperature index, mechanical strength

60 °C

Show Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746B

Vicat softening temperature

106 °C

Show Material materials with Vicat softening temperature of 106 °C

ASTM D 1525 | Rate B/50

Flammability

UL Recognized, 94HB Flame Class Rating | 1.52mm | UL 94

Rheological Properties

PropertyTemperatureValueComment

Melt viscosity

23.0 °C

1520 Pa·s

Show Material materials with Melt viscosity of 1520 Pa·s

ASTM D 3825 | 240°C, 100 sec⁻¹

Melt volume-flow rate

4 cm³/10min

Show Material materials with Melt volume-flow rate of 4 cm³/10min

ISO 1133 | 220°C/10.0 kg

Shrinkage

23.0 °C

0.7 - 0.9 %

Show Material materials with Shrinkage of 0.7 - 0.9 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Air Cabin Interiors,Electronic Components,Power Boat

Processing methods

Drying Temperature: 80-90°C, Drying Time: 5-4hrs, Drying Time (Cumulative): 24hrs, Maximum Moisture Content: 0.02-0.04%, Minimum Moisture Content: 0.04%, Barrel - Zone 1 Temperature: 190-220°C, Barrel - Zone 2 Temperature: 190-220°C, Barrel - Zone 3 Temperature: 190-220°C, Barrel - Zone 4 Temperature: 190-220°C, Adapter - Zone 5 Temperature: 195-220°C, Head - Zone 6 - Top Temperature: 195-220°C, Head - Zone 7 - Bottom Temperature: 195-220°C, Screw Speed: 20-60rpm, Extruder Feed Zone Temperature: 60-80°C, Mold Temperature: 40-90°C, Die Temperature: 195-220°C, Drying Temperature: 90-95°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0%, Melt Temperature: 210-240°C, Barrel - Zone 1 Temperature: 195-210°C, Barrel - Zone 2 Temperature: 200-220°C, Barrel - Zone 3 Temperature: 205-230°C, Barrel - Zone 4 Temperature: 210-235°C, Adapter Temperature: 200-225°C, Die Temperature: 210-240°C