SABIC® HDPE F00950 resin is a high molecular weight, high density polyethylene copolymer. The design of the product, molecular architecture and density, gives F00950 a good balance of easy extrusion and high melt strength with strong physical properties. SABIC® HDPE F00950 is typically used for production of thin films with good strength and rigidity. The material contains anti-oxidants. SABIC® HDPE F00950 resin is typically used for blown film extrusion and production of high strength grocery sacks, shopping bags and high quality thin films for multi wall sack liners and replacement for thin paper products. SABIC® HDPE F00950 can be extruded on conventional HMW-HDPE equipment with temperature settings between 200 and 220°C. Film properties have been measured at 25 µm films with a BUR = 4.Film has been produced on Kiefel IBC film blown line at 160 kg/h with a die of 150 mm, die gap of 1.2 mm and a frostline height of 150 cm (= 10D). This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

6 kN/m

Show Material materials with Tear strength of 6 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

20 kN/m

Show Material materials with Tear strength, transverse of 20 kN/m

ISO 6383-2

Technological properties

Property
Application areas

Grocery sacks, shopping bags, thin films for multi wall sack liners, replacement for thin paper products.