SABIC® HDPE F00952J resin is a high molecular weight, TNPP free high density polyethylene copolymer. The design of the product, molecular architecture and density, gives F00952J a good combination of easy extrusion and high melt strength with strong physical properties. Typical applications are thin films with excellent strength and rigidity. The material contains anti-oxidants. SABIC® HDPE F00952J resin is typically used for blown film extrusion and production of high strength grocery sacks, shopping bags and high quality thin films for multi wall sack liners and replacement for thin paper products. SABIC® HDPE F00952J can be extruded on conventional HMW-HDPE equipment at melt temperature settings between 200 and 220 °C. Film properties have been measured at 15 µm blown film with a BUR = 4. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

117.6 kN/m

Show Material materials with Tear strength of 117.6 kN/m

ASTM D1922

Tear strength, transverse

23.0 °C

588 kN/m

Show Material materials with Tear strength, transverse of 588 kN/m

ASTM D1922

Technological properties

Property
Application areas

Grocery sacks, shopping bags, thin films for multi wall sack liners, replacement for thin paper products.