Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94V-0/5VA rated. Elevated UL RTI rating.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Material materials with Density of 1.19 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.06 GPa

Show Material materials with Elastic modulus of 2.06 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

17 %

Show Material materials with Elongation of 17 %

ASTM D 638 | Type I, 5 mm/min

Elongation at yield

23.0 °C

2.4 %

Show Material materials with Elongation at yield of 2.4 %

ASTM D 638 | Type I, 5 mm/min

Flexural modulus

23.0 °C

2.26 GPa

Show Material materials with Flexural modulus of 2.26 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

63 MPa

Show Material materials with Flexural yield strength of 63 MPa

ISO 178 | 2 mm/min

Impact strength, Izod notched

23.0 °C

12 kJ/m²

Show Material materials with Impact strength, Izod notched of 12 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

23.0 °C

213 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 213 J/m

ASTM D 256

Tensile strength

23.0 °C

30 MPa

Show Material materials with Tensile strength of 30 MPa

ASTM D 638 | Type I, 5 mm/min

Yield strength

23.0 °C

37 MPa

Show Material materials with Yield strength of 37 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 9E-5 1/K

ASTM E 831 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

9.18E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 9.18E-5 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

75 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 75 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Relative temperature index, electrical

60 °C

Show Material materials with Relative temperature index, electrical of 60 °C

UL 746B

Relative temperature index, mechanical impact

60 °C

Show Material materials with Relative temperature index, mechanical impact of 60 °C

UL 746B

Relative temperature index, mechanical strength

60 °C

Show Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746B

Vicat softening temperature

93 °C

Show Material materials with Vicat softening temperature of 93 °C

ASTM D 1525 | Rate B/50

Flammability

UL Recognized, 94-5VA Flame Class Rating | 2.79mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

1 V

Show Material materials with Comparative tracking index of 1 V

UL 746A

Dielectric strength

23.0 °C

20 kV/mm

Show Material materials with Dielectric strength of 20 kV/mm

IEC 60243-1 | in oil, 3.2 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

7 g/10min

Show Material materials with Melt mass-flow rate of 7 g/10min

ISO 1133 | 220°C/5.0 kg

Melt viscosity

23.0 °C

320 Pa·s

Show Material materials with Melt viscosity of 320 Pa·s

ASTM D 3825 | 200°C, 1000 sec⁻¹

Melt volume-flow rate

40 cm³/10min

Show Material materials with Melt volume-flow rate of 40 cm³/10min

ISO 1133 | 220°C/10.0 kg

Shrinkage

23.0 °C

0.5 - 0.7 %

Show Material materials with Shrinkage of 0.5 - 0.7 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Aerospace,Air Cabin Interiors,Air Conditioning,ATM/Ticket Machine,Audio,Auto Aftermarket,Building Accessory,Building/Construction Sheet,Coffee Maker/Espresso Machine,Conveyor,Data Management,Data Transfer,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Food Processor,Headliner,Heavy Vehicles,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Monitoring and Imaging,Non-LED Lighting,Oil/Gas,Personal Computing,Photovoltaic Components,Pump,Refrigerator,Renal and Blood Handling,Security/Detection,Small Appliance,Surgical Devices,Vacuum Cleaner,Vending Machine,Washing Machine,Wireless Communications,Wiring Devices

Processing methods

Drying Temperature: 80-90°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.1%, Melt Temperature: 205-230°C, Nozzle Temperature: 205-230°C, Front - Zone 3 Temperature: 205-220°C, Middle - Zone 2 Temperature: 200-210°C, Rear - Zone 1 Temperature: 170-180°C, Mold Temperature: 50-70°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm