LEXAN™ Resin HF1110

Want to keep this datasheet? Save it now in your required format

Description

General purpose grade. Good clarity, heat resistance, property retention and dimensional stability.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Material materials with Density of 1.2 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.1 %

Show Material materials with Water absorption of 0.1 %

ASTM D 570 | 24 Hours

Water absorption, equilibrium

100.0 °C

0.58 %

Show Material materials with Water absorption, equilibrium of 0.58 %

ASTM D 570 | ASTM D 570

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

120 %

Show Material materials with Elongation of 120 %

ASTM D 638 | Type I, 50 mm/min

Flexural modulus

23.0 °C

2.3 GPa

Show Material materials with Flexural modulus of 2.3 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural yield strength

23.0 °C

93 MPa

Show Material materials with Flexural yield strength of 93 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Impact strength, Izod notched, ASTM

23.0 °C

640 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 640 J/m

ASTM D 256

Tensile strength

23.0 °C

65 MPa

Show Material materials with Tensile strength of 65 MPa

ASTM D 638 | Type I, 50 mm/min

Yield strength

23.0 °C

62 MPa

Show Material materials with Yield strength of 62 MPa

ASTM D 638 | Type I, 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

126 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 126 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B

Relative temperature index, mechanical impact

130 °C

Show Material materials with Relative temperature index, mechanical impact of 130 °C

UL 746B

Relative temperature index, mechanical strength

130 °C

Show Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B

Flammability

UL Recognized, 94V-2 Flame Class Rating | 1.09mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

2 V

Show Material materials with Comparative tracking index of 2 V

UL 746A

Optical

PropertyValueComment

Haze

1 %

Show Material materials with Haze of 1 %

ASTM D 1003 | 2.54 mm

Transmission

88 %

Show Material materials with Transmission of 88 %

ASTM D 1003 | 2.54 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

25 g/10min

Show Material materials with Melt mass-flow rate of 25 g/10min

ASTM D 1238 | 300°C/1.2 kg

Shrinkage

23.0 °C

0.5 - 0.7 %

Show Material materials with Shrinkage of 0.5 - 0.7 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Amusement Machine,ATM/Ticket Machine,Audio,Auto Aftermarket,Coffee Maker/Espresso Machine,Cooking Range,Data Management,Data Transfer,Dishwasher,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Food Processor,Forward Lighting,Fused Deposition Modeling (FDM),Heavy Vehicles,Industrial Material Handling,Infotainment/Telematic,Lab Ware and Clinical Diagnostics,Laundry Dryer,Medical Device,Meter Gas,Monitoring and Imaging,Non-LED Lighting,Overhead,Personal Care,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Photo/Video Camera,Power Manangement,Rear/Signal Lighting,Recreational Vehicle,Respiratory,Small Appliance,Surgical Devices,Vacuum Cleaner,Vending Machine,Washing Machine,Watch/Jewelry,Wearables,Wireless Communications,Wiring Devices

Processing methods

Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 270-295°C, Nozzle Temperature: 265-290°C, Front - Zone 3 Temperature: 270-295°C, Middle - Zone 2 Temperature: 260-280°C, Rear - Zone 1 Temperature: 250-270°C, Mold Temperature: 70-95°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm