SABIC® LDPE HP0824NDF

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE HP0824NDF is a grade typically used in foam applications. It is without slip and anti-block additives. This grades is ideally suitable for crosslink- and non-crosslink foaming processes using both physical and chemical blowing agents.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Crystallization temperature

97 °C

Show Material materials with Crystallization temperature of 97 °C

ISO 11357-3

Melting point

111 °C

Show Material materials with Melting point of 111 °C

SABIC method

Vicat softening temperature

97 °C

Show Material materials with Vicat softening temperature of 97 °C

ASTM D1525

Technological properties

Property
Application areas

Foam Extrusion,Footwear,Packaging,Automotive ,Foam