SABIC® LDPE HP20023

Want to keep this datasheet? Save it now in your required format

Description

HP20023 is an additive free low density polyethylene grade with high melt flow, offering good processability and capability to accept high pigment loading during compounding.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

45 [-]

Show Material materials with Hardness, Shore D of 45 [-]

ISO 868

Impact strength, Izod notched, ASTM

23.0 °C

500 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 500 J/m

ASTM D256

Thermal

PropertyValueComment

Crystallization temperature

98 °C

Show Material materials with Crystallization temperature of 98 °C

ISO 11357-3

Melting point

112 °C

Show Material materials with Melting point of 112 °C

SABIC method

Vicat softening temperature

92 °C

Show Material materials with Vicat softening temperature of 92 °C

ASTM D1525

Technological properties

Property
Application areas

Caps & closures,Masterbatch,Houseware & appliances