SABIC® LDPE HP4023WN

Want to keep this datasheet? Save it now in your required format

Description

HP4023WN is an antioxidant free low density polyethylene grade suitable for producing general-purpose films. It contains slip and antiblock additives. It gives excellent processability and optical properties with good mechanical properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyValueComment

Vicat softening temperature

91 °C

Show Material materials with Vicat softening temperature of 91 °C

ASTM D1525

Optical

PropertyValueComment

Haze

7 %

Show Material materials with Haze of 7 %

ASTM D1003

Technological properties

Property
Application areas

Blown film