SABIC® LDPE HP7023

Want to keep this datasheet? Save it now in your required format

Description

HP7023 is a Low Density Polyethylene grade that offers a unique combination of consistent processability, flexibility and toughness. Articles manufactured from HP7023 exhibits excellent impact strength, low shrinkage and good gloss.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

80 %

Show Material materials with Elongation of 80 %

ASTM D638

Hardness, Shore D

23.0 °C

43 [-]

Show Material materials with Hardness, Shore D of 43 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

490 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 490 J/m

ASTM D 256

Tensile strength

23.0 °C

10.5 MPa

Show Material materials with Tensile strength of 10.5 MPa

ASTM D638

Yield strength

23.0 °C

9 MPa

Show Material materials with Yield strength of 9 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

89 °C

Show Material materials with Vicat softening temperature of 89 °C

ASTM D1525

Rheological Properties

PropertyValueComment

Melt mass-flow rate

7 g/10min

Show Material materials with Melt mass-flow rate of 7 g/10min

ASTM D1238 | 190°C/2.16 kg

Technological properties

Property
Application areas

Caps & closures,Masterbatch