Description

PC/ASA flame retardant, excellent weatherability.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.17 g/cm³

Show Material materials with Density of 1.17 g/cm³

ISO 1183

Water absorption

23.0 °C

0.2 %

Show Material materials with Water absorption of 0.2 %

ISO 62 | 23°C, 50% RH

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.59 GPa

Show Material materials with Elastic modulus of 2.59 GPa

ASTM D 638 | 5 mm/min

Elongation at yield

23.0 °C

4.2 %

Show Material materials with Elongation at yield of 4.2 %

ASTM D 638 | Type I, 5 mm/min

Flexural modulus

23.0 °C

2.51 GPa

Show Material materials with Flexural modulus of 2.51 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

93 MPa

Show Material materials with Flexural yield strength of 93 MPa

ISO 178 | 2 mm/min

Impact strength, Charpy notched

23.0 °C

15 kJ/m²

Show Material materials with Impact strength, Charpy notched of 15 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

9 kJ/m²

Show Material materials with Impact strength, Izod notched of 9 kJ/m²

ISO 180/1A

23.0 °C

12 - 17 kJ/m²

Show Material materials with Impact strength, Izod notched of 12 - 17 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

23.0 °C

385 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 385 J/m

ASTM D 256

Tensile strength

23.0 °C

66 MPa

Show Material materials with Tensile strength of 66 MPa

ASTM D 638 | Type I, 5 mm/min

Yield strength

23.0 °C

59 MPa

Show Material materials with Yield strength of 59 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 6.9E-5 1/K

ISO 11359-2 | -30°C to 80°C

Coefficient of thermal expansion, transverse

23.0 °C

7.5E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 7.5E-5 1/K

ISO 11359-2 | 23°C to 80°C

Heat deflection temperature, 1.80 MPa

88 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 88 °C

ISO 75/Ae | 1.8 MPa

Vicat softening temperature

104 °C

Show Material materials with Vicat softening temperature of 104 °C

ISO 306 | Rate B/120

Flammability

UL Compliant, 94V-0 Flame Class Rating | 2mm | UL 94 by SABIC-IP

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

13 cm³/10min

Show Material materials with Melt volume-flow rate of 13 cm³/10min

ISO 1133 | 260°C/2.16 kg

Shrinkage

23.0 °C

0.4 - 0.6 %

Show Material materials with Shrinkage of 0.4 - 0.6 %

SABIC method

Technological properties

Property
Application areas

ATM/Ticket Machine,Audio,Building Element,Building/Construction Sheet,Circuit Protection,Data Transfer,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,LED Lighting,Medical Device,Meter Water,Personal Computing,Photo/Video Camera,Pump,Refrigerator,Security/Detection,Small Appliance,Surgical Devices,Swimming Pool/Spa,Vacuum Cleaner,Wireless Communications,Wiring Devices,Wire & cable

Processing methods

Drying Temperature: 80-90°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 230-270°C, Nozzle Temperature: 220-260°C, Front - Zone 3 Temperature: 230-270°C, Middle - Zone 2 Temperature: 220-260°C, Rear - Zone 1 Temperature: 200-230°C, Hopper Temperature: 60-80°C, Mold Temperature: 50-70°C