SABIC® PMMA IN20HR

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PMMA IN20HR is a PMMA grade with good heat resistance property suitable for extrusion and injection molding applications targeting unexposed applications to ultraviolet radiation. The grade is available in pellet form.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Material materials with Density of 1.19 g/cm³

ISO 1183

Water absorption

23.0 °C

0.3 %

Show Material materials with Water absorption of 0.3 %

ISO 62 | 24 Hours

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.3 GPa

Show Material materials with Elastic modulus of 3.3 GPa

ISO 527

Elongation

23.0 °C

6 %

Show Material materials with Elongation of 6 %

ISO 527

Flexural modulus

23.0 °C

3.3 GPa

Show Material materials with Flexural modulus of 3.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

140 MPa

Show Material materials with Flexural strength of 140 MPa

ISO 178

Hardness, Rockwell M

23.0 °C

101 [-]

Show Material materials with Hardness, Rockwell M of 101 [-]

ISO 2039

Impact strength, Charpy notched

23.0 °C

1.4 kJ/m²

Show Material materials with Impact strength, Charpy notched of 1.4 kJ/m²

ISO 179

Impact strength, Charpy unnotched

23.0 °C

20 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m²

ISO 179

Tensile strength

23.0 °C

77 MPa

Show Material materials with Tensile strength of 77 MPa

ISO 527

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion, transverse

23.0 °C

6E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 6E-5 1/K

ASTM D 696 | -30°C to 30°C

Heat deflection temperature, 1.80 MPa

100 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 100 °C

ISO 75-1&2 | 1.8 MPa

Thermal conductivity

23.0 °C

0.2 W/(m·K)

Show Material materials with Thermal conductivity of 0.2 W/(m·K)

ASTM C177

Vicat softening temperature

107 °C

Show Material materials with Vicat softening temperature of 107 °C

ISO 306 | B50

Optical

PropertyValueComment

Haze

0.3 %

Show Material materials with Haze of 0.3 %

ISO 14782

Luminous transmittance

93 [-]

Show Material materials with Luminous transmittance of 93 [-]

ISO 13468

Refractive index

1.49 [-]

Show Material materials with Refractive index of 1.49 [-]

ISO 489

Rheological Properties

PropertyValueComment

Melt mass-flow rate

2 g/10min

Show Material materials with Melt mass-flow rate of 2 g/10min

ISO 1133 | 230°C/3.16 kg

Technological properties

Property
Application areas

Lighting