CYCOLAC™ Resin INP108

Want to keep this datasheet? Save it now in your required format

Description

ABS, powder, medium impact. FDA compliant (part use must be at room temperature or below).

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.35 g/cm³

Show Material materials with Bulk density of 0.35 g/cm³

ASTM D 1895

Density

23.0 °C

1 g/cm³

Show Material materials with Density of 1 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

58 [-]

Show Material materials with Hardness, Shore D of 58 [-]

ISO 868

Technological properties

Property
Application areas

Building/Construction Sheet,Thermoplastic