Description

High heat AMSAN pellets.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.09 g/cm³

Show Material materials with Density of 1.09 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

3.62 GPa

Show Material materials with Flexural modulus of 3.62 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

58 MPa

Show Material materials with Flexural yield strength of 58 MPa

ISO 178 | 2 mm/min

Impact strength, Charpy notched

23.0 °C

1 kJ/m²

Show Material materials with Impact strength, Charpy notched of 1 kJ/m²

ISO 179/2C

Impact strength, Izod notched

-30.0 °C

1 kJ/m²

Show Material materials with Impact strength, Izod notched of 1 kJ/m²

ISO 180/1A

23.0 °C

3 kJ/m²

Show Material materials with Impact strength, Izod notched of 3 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

-30.0 °C

13 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 13 J/m

ASTM D 256

23.0 °C

19 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 19 J/m

ASTM D 256

Unlock all property charts

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

100 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 100 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Vicat softening temperature

118 °C

Show Material materials with Vicat softening temperature of 118 °C

ISO 306 | Rate B/120

Rheological Properties

PropertyValueComment

Melt mass-flow rate

21 g/10min

Show Material materials with Melt mass-flow rate of 21 g/10min

ISO 1133 | 220°C/10.0 kg

Technological properties

Property
Application areas

Cladding/Roof