Low flow polycarbonate resin with mold release. FDA food contact compliant. Available in limited transparent tints, limited package types, and must meet minimum order quantity requirements.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Material materials with Density of 1.19 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.15 %

Show Material materials with Water absorption of 0.15 %

ISO 62 | 23°C, 50% RH

Water absorption, equilibrium

23.0 °C

0.35 %

Show Material materials with Water absorption, equilibrium of 0.35 %

ASTM D 570

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.31 GPa

Show Material materials with Elastic modulus of 2.31 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

135 %

Show Material materials with Elongation of 135 %

ASTM D 638 | Type I, 50 mm/min

Elongation at yield

23.0 °C

7 %

Show Material materials with Elongation at yield of 7 %

ASTM D 638 | Type I, 50 mm/min

Flexural modulus

23.0 °C

2.3 GPa

Show Material materials with Flexural modulus of 2.3 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

90 MPa

Show Material materials with Flexural yield strength of 90 MPa

ISO 178 | 2 mm/min

Impact strength, Charpy notched

23.0 °C

95 kJ/m²

Show Material materials with Impact strength, Charpy notched of 95 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

10 kJ/m²

Show Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A

23.0 °C

65 kJ/m²

Show Material materials with Impact strength, Izod notched of 65 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

-30.0 °C

139 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 139 J/m

ASTM D 256

23.0 °C

850 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 850 J/m

ASTM D 256

Unlock all property charts

Impact strength, Izod unnotched, ASTM

23.0 °C

3204 J/m

Show Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m

ASTM D 4812

Tensile strength

23.0 °C

68 MPa

Show Material materials with Tensile strength of 68 MPa

ASTM D 638 | Type I, 50 mm/min

Yield strength

23.0 °C

63 MPa

Show Material materials with Yield strength of 63 MPa

ASTM D 638 | Type I, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 6E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

6E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 6E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

132 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 132 °C

ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed

Vicat softening temperature

154 °C

Show Material materials with Vicat softening temperature of 154 °C

ASTM D 1525 | Rate B/50

Optical

PropertyValueComment

Haze

1 %

Show Material materials with Haze of 1 %

ASTM D 1003 | 2.54 mm

Refractive index

1.59 [-]

Show Material materials with Refractive index of 1.59 [-]

ASTM D542

Transmission

88 %

Show Material materials with Transmission of 88 %

ASTM D 1003 | 2.54 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

7 g/10min

Show Material materials with Melt mass-flow rate of 7 g/10min

ASTM D 1238 | 300°C/1.2 kg

Melt volume-flow rate

6 cm³/10min

Show Material materials with Melt volume-flow rate of 6 cm³/10min

ISO 1133 | 300°C/1.2 kg

Shrinkage

23.0 °C

0.5 - 0.7 %

Show Material materials with Shrinkage of 0.5 - 0.7 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Sunglasses

Processing methods

Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 48hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 310-330°C, Nozzle Temperature: 305-325°C, Front - Zone 3 Temperature: 310-330°C, Middle - Zone 2 Temperature: 300-320°C, Rear - Zone 1 Temperature: 290-310°C, Mold Temperature: 80-115°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 40-70rpm, Shot to Cylinder Size: 40-60%, Vent Depth: 0.025-0.076mm