SABIC® LLDPE M500026

Want to keep this datasheet? Save it now in your required format

Description

M500026 is a Linear Low Density Polyethylene grade with narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excellent flow properties with better low temperature toughness, stress crack resistance and gloss.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.93 g/cm³

Show Material materials with Density of 0.93 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

55 [-]

Show Material materials with Hardness, Shore D of 55 [-]

ISO 868

Impact strength, Izod notched, ASTM

23.0 °C

450 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 450 J/m

ASTM D256A

Technological properties

Property
Application areas

Thin wall packaging,Masterbatch,Houseware & appliances