SABIC® HDPE M80064

Want to keep this datasheet? Save it now in your required format

Description

M80064 is a High Density Polyethylene grade with narrow molecular weight distribution suitable for injection molding applications. It has been designed to give good rigidity, toughness and low warpage.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Material materials with Density of 0.96 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.65 GPa

Show Material materials with Flexural modulus of 1.65 GPa

ASTM D 790

Flexural strength

23.0 °C

42 MPa

Show Material materials with Flexural strength of 42 MPa

ASTM D790

Hardness, Shore D

23.0 °C

62 [-]

Show Material materials with Hardness, Shore D of 62 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

75 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 75 J/m

ASTM D256

Tensile strength

23.0 °C

18 MPa

Show Material materials with Tensile strength of 18 MPa

ASTM D638

Yield strength

23.0 °C

26 MPa

Show Material materials with Yield strength of 26 MPa

ASTM D638

Thermal

PropertyValueComment

Vicat softening temperature

125 °C

Show Material materials with Vicat softening temperature of 125 °C

ASTM D1525

Technological properties

Property
Application areas

Multi purpose injection moulding,Containers & pails