Description

SABIC HDPE P4200RT is a high-density polyethylene (HDPE) with high melt viscosity for extrusion. The product provides excellent stress crack resistance properties (ESCR) combined with very good long-term hydrostatic strength, high heat & extremely high extraction stability. It is designed to fulfill all the requirements of DIN 16833 / ISO 24033 for PE-RT Type II.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.95 g/cm³

Show Material materials with Density of 0.95 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation at yield

23.0 °C

8 %

Show Material materials with Elongation at yield of 8 %

ISO 527-2

Hardness, Shore D

23.0 °C

59 [-]

Show Material materials with Hardness, Shore D of 59 [-]

ISO 868

Impact strength, Charpy notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179

23.0 °C

24 kJ/m²

Show Material materials with Impact strength, Charpy notched of 24 kJ/m²

ISO 179

Yield strength

23.0 °C

22 MPa

Show Material materials with Yield strength of 22 MPa

ISO 527-2

Thermal

PropertyValueComment

Vicat softening temperature

70 °C

Show Material materials with Vicat softening temperature of 70 °C

ISO 306 | 50N (VST/B)

Technological properties

Property
Application areas

Pipe,Ground floor heating