SABIC® HDPE 5510 10000 (black) is a grade, which has a high density (class MRS 8 - PE 80) and a bimodal distribution of the molecular mass. An universal grade for pipe extrusion which, due to a keen combination of properties, is particularly suitable for drinking water and waste water piping. It is also used for the manufacture of chemical apparatus and containers. This material meets (inter)national standards for use in drinking water and wastewater piping.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Material materials with Density of 0.96 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.85 GPa

Show Material materials with Elastic modulus of 0.85 GPa

ASTM D638

Elongation at yield

23.0 °C

8 %

Show Material materials with Elongation at yield of 8 %

ISO 527-1/-2

Hardness, Shore D

23.0 °C

59 [-]

Show Material materials with Hardness, Shore D of 59 [-]

ISO 868

Impact strength, Charpy notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179

23.0 °C

24 kJ/m²

Show Material materials with Impact strength, Charpy notched of 24 kJ/m²

ISO 179

Yield strength

23.0 °C

22 MPa

Show Material materials with Yield strength of 22 MPa

ISO 527-1/-2

Thermal

PropertyValueComment

Vicat softening temperature

70 °C

Show Material materials with Vicat softening temperature of 70 °C

ISO 306 | 50 N (VST/B)