Description

SABIC® SUPEER™ P8200RT is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. SUPEER™ P8200RT performs well in a wide range of pipe applications with excellent long-term hydrostatic strength, combined with good surface and superior processibility. It is designed to fulfill all the requirements of DIN 16833 / ISO 24033 for PE-RT Type II.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

60 [-]

Show Material materials with Hardness, Shore D of 60 [-]

ASTM D2240 | 1 second

Thermal

PropertyValueComment

Melting point

128 °C

Show Material materials with Melting point of 128 °C

SABIC method

Vicat softening temperature

121 °C

Show Material materials with Vicat softening temperature of 121 °C

ASTM D1525