SABIC® LDPE PCG00

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LDPE grades for healthcare applications are produced under controlled conditions resulting in high product quality, consistency and a high level of purity. SABIC® LDPE PCG00 is an additive-free grade produced using SABIC’s proprietary high pressure Clean Tubular Reactor (CTR®) which typically ensures grades with high purity. It is typically used for semi-rigid containers obtained by Blow Fill Seal (BFS) process and medical films. Compliance to Regulations SABIC® LDPE PCG00 complies with the relevant monographs of the European Pharmacopoeia (EP) and the United States Pharmacopoeia (USPVI).

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

1 [-]

Show Material materials with Coefficient of friction of 1 [-]

ASTM D1894

Density

23.0 °C

0.93 g/cm³

Show Material materials with Density of 0.93 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

35 kN/m

Show Material materials with Tear strength of 35 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

45 kN/m

Show Material materials with Tear strength, transverse of 45 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

8 %

Show Material materials with Haze of 8 %

ASTM D1003

Technological properties

Property
Application areas

It is typically used for semi-rigid containers obtained by Blow Fill Seal (BFS) process and medical films.