SABIC® LLDPE PCG61

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE PCG61 is a hexene-linear low density polyethylene typically used for healthcare applications. Films made from this resin exhibit good mechanical, optical and hottack properties. Typical application for SABIC® LLDPE PCG61 are pharmaceutical films, bags and pouches requiring good impact strength, tear resistance,optical performance andhottack properties. Film properties: Film of 50 µm and BUR = 2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2.7 mm. Compliance to RegulationsSABIC® LLDPE PCG61 complies with the relevant monographs of the European Pharmacopoeia (EP) and the United States Pharmacopoeia (USPVI).

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

100 kN/m

Show Material materials with Tear strength of 100 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

400 kN/m

Show Material materials with Tear strength, transverse of 400 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

13 %

Show Material materials with Haze of 13 %

ASTM D1003

Technological properties

Property
Application areas

Pharmaceutical films, bags and pouches requiring good impact strength, tear resistance,optical performance andhottack properties.