SABIC® PP QR6711K

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP QR6711K is a PP random grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity. This grade contains advanced clarifier & anti-static agent. SABIC® PP QR6711K has the following features: Consistent processability; Good stiffness; Exceptional clarity; Low thickness; Low warpage; Easy to flow; Better cycle time comparing to normal PP random copolymer grades; Less energy consumption.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.15 GPa

Show Material materials with Flexural modulus of 1.15 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

85 [-]

Show Material materials with Hardness, Rockwell L of 85 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

124 °C

Show Material materials with Vicat softening temperature of 124 °C

ASTM D1525

Technological properties

Property
Application areas

Caps & closures,Thin wall packaging,Containers & pails