SABIC® PP QR6731K

Want to keep this datasheet? Save it now in your required format

Description

SABIC® PP QR6731K is specially developed for producing injection molded & ISBM articles with very high clarity at low processing temperatures. This grade contains advance clarifier and anti-static agent. SABIC® PP QR6731K has following features: Consistent processability; Good stiffness; Exceptional clarity; Lower energy consumption and less cycle time due to low processing temperatures.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

1.05 GPa

Show Material materials with Flexural modulus of 1.05 GPa

ASTM D790 A

Hardness, Rockwell L

23.0 °C

94 [-]

Show Material materials with Hardness, Rockwell L of 94 [-]

ASTM D785

Thermal

PropertyValueComment

Vicat softening temperature

127 °C

Show Material materials with Vicat softening temperature of 127 °C

ASTM D1525

Technological properties

Property
Application areas

Caps & closures,Bottles & cans