SABIC® LLDPE R40039E

Want to keep this datasheet? Save it now in your required format

Description

R40039E is a linear low density polyethylene grade with elevated density and higher viscosity designed to provide excellent mechanical properties with high rigidity, toughness, good impact strength, low warpage as well as excellent internal and external surface finish. It is in pelletized form, UV-stabilized and has good stress cracking resistance which can be suitable for outdoor applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.94 g/cm³

Show Material materials with Density of 0.94 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural strength

23.0 °C

15 MPa

Show Material materials with Flexural strength of 15 MPa

ASTM D790

Hardness, Shore D

23.0 °C

69 [-]

Show Material materials with Hardness, Shore D of 69 [-]

ISO 868

Thermal

PropertyValueComment

Vicat softening temperature

119 °C

Show Material materials with Vicat softening temperature of 119 °C

ASTM D1525