SABIC® LLDPE R50035E

Want to keep this datasheet? Save it now in your required format

Description

R50035E is a Linear Low Density Polyethylene grade with balanced density and viscosity designed to provide excellent stress cracking resistance, good mechanical properties with high rigidity, toughness, and low warpage. R50035E is an antioxdant and UV stabilized grade in pellet form.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.94 g/cm³

Show Material materials with Density of 0.94 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

0.42 GPa

Show Material materials with Flexural modulus of 0.42 GPa

ASTM D790 A

Flexural strength

23.0 °C

13 MPa

Show Material materials with Flexural strength of 13 MPa

ASTM D790

Hardness, Shore D

23.0 °C

66 [-]

Show Material materials with Hardness, Shore D of 66 [-]

ISO 868

Thermal

PropertyValueComment

Vicat softening temperature

114 °C

Show Material materials with Vicat softening temperature of 114 °C

ASTM D1525