XENOY™ Resin RCX201

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.23 g/cm³

Show Material materials with Density of 1.23 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

200 %

Show Material materials with Elongation of 200 %

SABIC - Japan Method

Flexural modulus

23.0 °C

2.15 GPa

Show Material materials with Flexural modulus of 2.15 GPa

ASTM D 790

Flexural strength

23.0 °C

82 MPa

Show Material materials with Flexural strength of 82 MPa

ASTM D 790

Impact strength, Izod notched, ASTM

-30.0 °C

50 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 50 J/m

ASTM D 256

23.0 °C

392 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 392 J/m

ASTM D 256

Yield strength

23.0 °C

52 MPa

Show Material materials with Yield strength of 52 MPa

SABIC - Japan Method

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 6E-5 1/K

TMA | -30°C to 30°C

Heat deflection temperature, 1.80 MPa

130 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 130 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 - 0.8 %

Show Material materials with Shrinkage of 0.5 - 0.8 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Displays,Document Handling,Door Handle,Electronic Components,Exterior,Front Grille,Rear/Signal Lighting,Recreational Vehicle,Security/Detection