SABIC® COHERE™ S400

Want to keep this datasheet? Save it now in your required format

Description

SABIC® COHERE™ S400 is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. It performs well in high performance flexible packaging applications with excellent toughness, hot tack, hot seal, optical properties and shows enhanced cling force in protection film application.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.9 g/cm³

Show Material materials with Density of 0.9 g/cm³

ASTM D792

Thermal

PropertyValueComment

Melting point

96 °C

Show Material materials with Melting point of 96 °C

SABIC method

Optical

PropertyValueComment

Haze

0.5 %

Show Material materials with Haze of 0.5 %

ASTM D1003

Rheological Properties

PropertyValueComment

Melt mass-flow rate

3.5 g/10min

Show Material materials with Melt mass-flow rate of 3.5 g/10min

ASTM D1238 | 190°C/2.16 kg

Technological properties

Property
Application areas

Cast film