Description

SABIC® P1600A shows superior abrasion resistance, excellent chemical and corrosion resistance, easy processing ability, and good compatibility with HDPE pipes. Typical customer applications are mining and dredging application, a section of piping for use in transporting abrasive slurries requires pipeline with improved abrasion resistance.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.89 g/cm³

Show Material materials with Density of 0.89 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.06 GPa

Show Material materials with Elastic modulus of 0.06 GPa

ISO 527

Hardness, Shore A

23.0 °C

91 [-]

Show Material materials with Hardness, Shore A of 91 [-]

ISO 868

Impact strength, Charpy notched

23.0 °C

28 kJ/m²

Show Material materials with Impact strength, Charpy notched of 28 kJ/m²

ISO 179

Thermal

PropertyValueComment

Vicat softening temperature

53 °C

Show Material materials with Vicat softening temperature of 53 °C

ISO 306 | 10N (VST/A)

Rheological Properties

PropertyValueComment

Melt mass-flow rate

28.3 g/10min

Show Material materials with Melt mass-flow rate of 28.3 g/10min

ISO 1133 | 190°C/21.6 kg