XENOY™ Resin X2203

Want to keep this datasheet? Save it now in your required format

Description

Xenoy product that provides improved chemical resistance and impact performance versus previous generation X2202 product which is used in the market spaces such as soap dispenser, cleaning equipment, filter housing

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

2.64 GPa

Show Material materials with Flexural modulus of 2.64 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural yield strength

23.0 °C

100 MPa

Show Material materials with Flexural yield strength of 100 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Impact strength, Izod notched, ASTM

-20.0 °C

127 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 127 J/m

ASTM D 256

23.0 °C

209 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 209 J/m

ASTM D 256

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

90 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 90 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Rheological Properties

PropertyValueComment

Melt volume-flow rate

35 cm³/10min

Show Material materials with Melt volume-flow rate of 35 cm³/10min

ISO 1133 | 265°C/5.0 kg

Technological properties

Property
Application areas

Personal Care

Processing methods

Drying Temperature: 110°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 260-280°C, Nozzle Temperature: 255-275°C, Front - Zone 3 Temperature: 260-280°C, Middle - Zone 2 Temperature: 255-275°C, Rear - Zone 1 Temperature: 250-270°C, Mold Temperature: 65-95°C, Back Pressure: 0.3-0.6MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 50-80%, Vent Depth: 0.013-0.02mm