XYLEX™ Resin X7509HP

Want to keep this datasheet? Save it now in your required format

Description

PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HX7509HP.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Material materials with Density of 1.2 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.05 %

Show Material materials with Water absorption of 0.05 %

ISO 62 | 23°C, 50% RH

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.14 GPa

Show Material materials with Elastic modulus of 2.14 GPa

ASTM D 638 | 50 mm/min

Elongation

23.0 °C

135 %

Show Material materials with Elongation of 135 %

ASTM D 638 | Type I, 50 mm/min

Elongation at yield

23.0 °C

6.3 %

Show Material materials with Elongation at yield of 6.3 %

ASTM D 638 | Type I, 50 mm/min

Flexural modulus

23.0 °C

2.25 GPa

Show Material materials with Flexural modulus of 2.25 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

92 MPa

Show Material materials with Flexural strength of 92 MPa

ISO 178

Flexural yield strength

23.0 °C

95 MPa

Show Material materials with Flexural yield strength of 95 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Impact strength, Charpy notched

23.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A

23.0 °C

9 kJ/m²

Show Material materials with Impact strength, Izod notched of 9 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

-30.0 °C

70 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 70 J/m

ASTM D 256

23.0 °C

850 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 850 J/m

ASTM D 256

Unlock all property charts

Tensile strength

23.0 °C

63 MPa

Show Material materials with Tensile strength of 63 MPa

ASTM D 638 | Type I, 50 mm/min

Yield strength

23.0 °C

60 MPa

Show Material materials with Yield strength of 60 MPa

ASTM D 638 | Type I, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.04E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.04E-4 1/K

ASTM E 831 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

1.04E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.04E-4 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

106 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 106 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Vicat softening temperature

126 °C

Show Material materials with Vicat softening temperature of 126 °C

ASTM D 1525 | Rate B/50

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

12 g/10min

Show Material materials with Melt mass-flow rate of 12 g/10min

ASTM D 1238 | 265°C/2.16kgf

Melt volume-flow rate

11 cm³/10min

Show Material materials with Melt volume-flow rate of 11 cm³/10min

ISO 1133 | 265°C/2.16 kg

Shrinkage

23.0 °C

0.4 - 0.6 %

Show Material materials with Shrinkage of 0.4 - 0.6 %

SABIC method | 3.2 mm

Shrinkage, transverse

23.0 °C

0.5 - 0.7 %

Show Material materials with Shrinkage, transverse of 0.5 - 0.7 %

SABIC method

Technological properties

Property
Application areas

Auto Aftermarket,Bottles,Building Element,Data Transfer,Dishwasher,Displays,Document Handling,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Monitoring and Imaging,Non-LED Lighting,Personal Care,Personal Computing,Pharmaceutical Packaging & Drug Delivery,Rail Cabin Interiors,Renal and Blood Handling,Swimming Pool/Spa,Washing Machine,Wireless Communications,Wiring Devices

Processing methods

Drying Temperature: 65-80°C, Drying Time: 3-5hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-270°C, Nozzle Temperature: 250-270°C, Front - Zone 3 Temperature: 250-270°C, Middle - Zone 2 Temperature: 245-270°C, Rear - Zone 1 Temperature: 245-260°C, Mold Temperature: 45-60°C, Back Pressure: 0.1-0.5MPa, Screw Speed: 20-100rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.013-0.02mm