GELOY™ Resin XP4034

Want to keep this datasheet? Save it now in your required format

Description

PC/ASA. Excellent weatherability.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.15 g/cm³

Show Material materials with Density of 1.15 g/cm³

ISO 1183

Water absorption

23.0 °C

0.25 %

Show Material materials with Water absorption of 0.25 %

ISO 62 | 23°C, 50% RH

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.4 GPa

Show Material materials with Elastic modulus of 2.4 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

35 %

Show Material materials with Elongation of 35 %

ISO 527 | 50 mm/min

Elongation at yield

23.0 °C

4.5 %

Show Material materials with Elongation at yield of 4.5 %

ISO 527 | 50 mm/min

Flexural modulus

23.0 °C

2.5 GPa

Show Material materials with Flexural modulus of 2.5 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

80 MPa

Show Material materials with Flexural yield strength of 80 MPa

ISO 178 | 2 mm/min

Hardness, Ball Indentation

23.0 °C

98 MPa

Show Material materials with Hardness, Ball Indentation of 98 MPa

ISO 2039-1

Impact strength, Izod notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A

23.0 °C

33 kJ/m²

Show Material materials with Impact strength, Izod notched of 33 kJ/m²

ISO 180/1A

Tensile strength

23.0 °C

50 MPa

Show Material materials with Tensile strength of 50 MPa

ISO 527 | 50 mm/min

Yield strength

23.0 °C

57 MPa

Show Material materials with Yield strength of 57 MPa

ISO 527 | 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

100 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 100 °C

ISO 75/Ae | 1.8 MPa

Vicat softening temperature

109 °C

Show Material materials with Vicat softening temperature of 109 °C

ISO 306 | Rate B/120

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

15 cm³/10min

Show Material materials with Melt volume-flow rate of 15 cm³/10min

ISO 1133 | 260°C/5.0 kg

Shrinkage

23.0 °C

0.4 - 0.6 %

Show Material materials with Shrinkage of 0.4 - 0.6 %

SABIC method

Technological properties

Property
Application areas

Applique,Audio,Auto Aftermarket,Building Element,Cluster,Cowl Vent Grille,Data Management,Data Transfer,Document Handling,Door Handle,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exercise Equipment,Exterior Mirror,Exterior Trim,Exterior,Food Processor,Forward Lighting,Front Grille,Glove Box,Heavy Vehicles,Infotainment/Telematic,Interior,Lighting,Non-LED Lighting,Overhead,Personal Computing,Rear/Signal Lighting,Recreational Vehicle,Seat,Security/Detection,Spoiler,Trim,Wireless Communications

Processing methods

Drying Temperature: 90-105°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 260-275°C, Mold Temperature: 50-70°C