Delrin® 100TL NC010

Alternative and trade names
POM-SD
Want to keep this datasheet? Save it now in your required format

Description

Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades. Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.Delrin® 100TL is a high viscosity acetal homopolymer with1.5% PTFE micropowder.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.43 g/cm³

Show Material materials with Density of 1.43 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3 GPa

Show Material materials with Elastic modulus of 3 GPa

ISO 527-1/-2

Elongation

23.0 °C

35 %

Show Material materials with Elongation of 35 %

ISO 527-1/-2

Elongation at yield

23.0 °C

25 %

Show Material materials with Elongation at yield of 25 %

ISO 527-1/-2

Flexural modulus

23.0 °C

2.8 GPa

Show Material materials with Flexural modulus of 2.8 GPa

ISO 178

Impact strength, Charpy notched

-6.0 °C

8 kJ/m²

Show Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179/1eA

23.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

150 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 150 kJ/m²

ISO 179/1eU

Poisson's ratio

23.0 °C

0.37 [-]

Show Material materials with Poisson's ratio of 0.37 [-]

Yield strength

23.0 °C

71 MPa

Show Material materials with Yield strength of 71 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.1E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-4 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

1.1E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.1E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

158 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 158 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

95 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 95 °C

ISO 75-1/-2

Melting point

178 °C

Show Material materials with Melting point of 178 °C

ISO 11357-1/-3 | 18°F/min

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: 42 mm/min

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

2.4 g/10min

Show Material materials with Melt mass-flow rate of 2.4 g/10min

ISO 1133 | 190°C/2.16kg

Shrinkage

23.0 °C

1.8 %

Show Material materials with Shrinkage of 1.8 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1.7 %

Show Material materials with Shrinkage, transverse of 1.7 %

ISO 294-4, 2577

Technological properties

Property
Fillers

PTFE

Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 215°C, Min. melt temperature: 210°C, Max. melt temperature: 220°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 90-110MPa, Hold pressure time: 8s/mm