Elvamide® 8061

Want to keep this datasheet? Save it now in your required format

Description

DuPont Elvamide® nylon multipolymer resins are a family of unique polymers having outstanding abrasion resistance, high tensile strength and elongation, and excellent adhesion to nylon yarns. Important benefits of DuPont Elvamide® are:Excellent adhesion to nylon yarn Readily applied from solutions in low cost, quick evaporating alcohols High melting point prevents “gumming-up” at high needle temperatures frequently encountered in high speed sewing Only 4% to 10% Elvamide® is required to give excellent bonding, with consistent quality Elvamide®8061 is a general purpose nylon multipolymer resin combining good solubility, abrasion resistance and toughness.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Water absorption

23.0 °C

3.1 %

Show Material materials with Water absorption of 3.1 %

Sim. to ISO 62 | Immersion 24h

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

320 %

Show Material materials with Elongation of 320 %

ASTM D 638

Flexural modulus

23.0 °C

0.95 GPa

Show Material materials with Flexural modulus of 0.95 GPa

ASTM D 790

Hardness, Rockwell R

23.0 °C

71 [-]

Show Material materials with Hardness, Rockwell R of 71 [-]

ASTM D 785

Tensile strength

23.0 °C

51 MPa

Show Material materials with Tensile strength of 51 MPa

ASTM D 638

Thermal

PropertyValueComment

Melting point

156 °C

Show Material materials with Melting point of 156 °C

ISO 11357-1/-3 | 18°F/min

Technological properties

Property