Description

Common features of Minlon® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness /toughness, good high temperature performance, good chemical resistance, paintability, dimensional stability and low warpage. Grades with improved electrical and flammability properties are available within the Zytel® nylon resin product line. In addition, Minlon® nylon resin is available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses.The good melt stability of Minlon® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.Minlon® nylon resin typically is used in demanding applications in the automotive, electrical, electronic, domestic appliances and construction industries.Minlon® 73M40 NC010 is a 40% mineral reinforced, heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.45 g/cm³

Show Material materials with Density of 1.45 g/cm³

ISO 1183

Water absorption

23.0 °C

5.4 %

Show Material materials with Water absorption of 5.4 %

Sim. to ISO 62 | 80mil

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

6 GPa

Show Material materials with Elastic modulus of 6 GPa

ISO 527-1/-2

Elongation

23.0 °C

10 %

Show Material materials with Elongation of 10 %

ISO 527-1/-2

Flexural modulus

23.0 °C

5.9 GPa

Show Material materials with Flexural modulus of 5.9 GPa

ISO 178

Flexural strength

23.0 °C

135 MPa

Show Material materials with Flexural strength of 135 MPa

ISO 178

Impact strength, Charpy notched

-6.0 °C

4 kJ/m²

Show Material materials with Impact strength, Charpy notched of 4 kJ/m²

ISO 179/1eA

23.0 °C

5.5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.5 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-6.0 °C

95 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 95 kJ/m²

ISO 179/1eU

23.0 °C

130 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 130 kJ/m²

ISO 179/1eU

Unlock all property charts

Impact strength, Izod unnotched

-30.0 °C

4 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 4 kJ/m²

ISO 180/1A

23.0 °C

5 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 5 kJ/m²

ISO 180/1A

Unlock all property charts

Poisson's ratio

23.0 °C

0.35 [-]

Show Material materials with Poisson's ratio of 0.35 [-]

Tensile strength

23.0 °C

87 MPa

Show Material materials with Tensile strength of 87 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6.5E-5 1/K

Show Material materials with Coefficient of thermal expansion of 6.5E-5 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

7.5E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 7.5E-5 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

196 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 196 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

110 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 110 °C

ISO 75-1/-2

Melting point

221 °C

Show Material materials with Melting point of 221 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

65 °C

Show Material materials with Relative temperature index, electrical of 65 °C

UL 746B | 30mil

Relative temperature index, mechanical impact

65 °C

Show Material materials with Relative temperature index, mechanical impact of 65 °C

UL 746B | 30mil

Relative temperature index, mechanical strength

65 °C

Show Material materials with Relative temperature index, mechanical strength of 65 °C

UL 746B | 30mil

Specific heat capacity

23.0 °C

1940 J/(kg·K)

Show Material materials with Specific heat capacity of 1940 J/(kg·K)

of melt

Vicat softening temperature

210 °C

Show Material materials with Vicat softening temperature of 210 °C

ISO 306 | 90°F/h, 11 lbf

Flammability

Burning Behav. at thickness h: HB class, Thickness tested: 0.85 mm, UL recognition: yes -, FMVSS Class: SE -

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.8 %

Show Material materials with Shrinkage of 0.8 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

0.8 %

Show Material materials with Shrinkage, transverse of 0.8 %

ISO 294-4, 2577

Technological properties

Property
Fillers

40% Mineral Powder

Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 270°C, Min. melt temperature: 260°C, Max. melt temperature: 280°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C