Description

Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness...

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.57 g/cm³

Show Material materials with Density of 1.57 g/cm³

ISO 1183

Water absorption

23.0 °C

0.6 %

Show Material materials with Water absorption of 0.6 %

Sim. to ISO 62 | Immersion 24h

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

10 GPa

Show Material materials with Elastic modulus of 10 GPa

ISO 527-1/-2

Elongation

23.0 °C

2.6 %

Show Material materials with Elongation of 2.6 %

ISO 527-1/-2

Impact strength, Charpy notched

-40.0 °C

12 kJ/m²

Show Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO 179/1eA

-6.0 °C

12 kJ/m²

Show Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO 179/1eA

23.0 °C

12 kJ/m²

Show Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-40.0 °C

50 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

ISO 179/1eU

-6.0 °C

50 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

ISO 179/1eU

23.0 °C

60 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

ISO 179/1eU

Unlock all property charts

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Tensile strength

23.0 °C

170 MPa

Show Material materials with Tensile strength of 170 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.1E-5 1/K

ISO 11359-1/-2 | 23 - 55°C

Coefficient of thermal expansion, transverse

23.0 °C

1.1E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.1E-4 1/K

ISO 11359-1/-2 | 55 - 160°C

Heat deflection temperature, 1.80 MPa

240 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 240 °C

ISO 75-1/-2

Melting point

262 °C

Show Material materials with Melting point of 262 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

115 °C

Show Material materials with Relative temperature index, mechanical impact of 115 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

120 °C

Show Material materials with Relative temperature index, mechanical strength of 120 °C

UL 746B | 120mil

Flammability

Burning Behav. at 60mil nom. thickn.: V-0 class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: V-0 class, Thickness tested: 0.75 mm, UL recognition: yes -, Burning Behav. 5V at thickness h: 5VA class, Thickness tested: 1.5 mm, UL recognition: yes -, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

275 V

Show Material materials with Comparative tracking index of 275 V

IEC 60112

Dielectric strength

23.0 °C

24 kV/mm

Show Material materials with Dielectric strength of 24 kV/mm

IEC 60243-1

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Material materials with Volume resistivity of 1.00E+15 Ω·cm

min. | IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Material materials with Shrinkage of 0.3 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

0.8 %

Show Material materials with Shrinkage, transverse of 0.8 %

ISO 294-4, 2577

Technological properties

Property
Fillers

25% Glass Fiber

Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm