Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including most flame retardant grades, offer the ability to be coloured. The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.Zytel® 79G13HSLBK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.21 g/cm³

Show Material materials with Density of 1.21 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

5.1 GPa

Show Material materials with Elastic modulus of 5.1 GPa

ISO 527-1/-2

Elongation

23.0 °C

4 %

Show Material materials with Elongation of 4 %

ISO 527-1/-2

Impact strength, Charpy notched

-6.0 °C

6 kJ/m²

Show Material materials with Impact strength, Charpy notched of 6 kJ/m²

ISO 179/1eA

23.0 °C

8 kJ/m²

Show Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-6.0 °C

59 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 59 kJ/m²

ISO 179/1eU

23.0 °C

67 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 67 kJ/m²

ISO 179/1eU

Unlock all property charts

Impact strength, Izod unnotched

23.0 °C

7.5 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 7.5 kJ/m²

ISO 180/1A

Poisson's ratio

23.0 °C

0.35 [-]

Show Material materials with Poisson's ratio of 0.35 [-]

Tensile strength

23.0 °C

115 MPa

Show Material materials with Tensile strength of 115 MPa

ISO 527-1/-2

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

260 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 260 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

240 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 240 °C

ISO 75-1/-2

Melting point

262 °C

Show Material materials with Melting point of 262 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

120 °C

Show Material materials with Relative temperature index, electrical of 120 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

105 °C

Show Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

120 °C

Show Material materials with Relative temperature index, mechanical strength of 120 °C

UL 746B | 120mil

Flammability

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.8 mm, UL recognition: yes -, FMVSS Class: B -, Burning rate, Thickness 1 mm: 24 mm/min

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Material materials with Shrinkage of 0.5 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

0.8 %

Show Material materials with Shrinkage, transverse of 0.8 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 80°C, Min. mold temperature: 50°C, Max. mold temperature: 100°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C