Zytel® FN718 BK230A

Alternative and trade names
PA66-F
Want to keep this datasheet? Save it now in your required format

Description

Zytel® FN718 BK230A is a flexible polyamide 66 resin.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Material materials with Density of 1.04 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.9 GPa

Show Material materials with Elastic modulus of 0.9 GPa

ISO 527-1/-2

Elongation

23.0 °C

500 %

Show Material materials with Elongation of 500 %

min. | ISO 527-1/-2

Flexural modulus

23.0 °C

0.9 GPa

Show Material materials with Flexural modulus of 0.9 GPa

ISO 178

Impact strength, Charpy notched

-40.0 °C

30 kJ/m²

Show Material materials with Impact strength, Charpy notched of 30 kJ/m²

ISO 179/1eA

23.0 °C

105 kJ/m²

Show Material materials with Impact strength, Charpy notched of 105 kJ/m²

ISO 179/1eA

Impact strength, Izod unnotched

-40.0 °C

25 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 25 kJ/m²

ISO 180/1A

23.0 °C

95 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 95 kJ/m²

ISO 180/1A

Unlock all property charts

Poisson's ratio

23.0 °C

0.45 [-]

Show Material materials with Poisson's ratio of 0.45 [-]

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

68 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 68 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

50 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 50 °C

ISO 75-1/-2

Melting point

263 °C

Show Material materials with Melting point of 263 °C

ISO 11357-1/-3 | 18°F/min

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 285°C, Min. melt temperature: 275°C, Max. melt temperature: 295°C, Mold Temperature Optimum: 60°C, Min. mold temperature: 40°C, Max. mold temperature: 80°C