Zytel® EFE1068 NC010T

Alternative and trade names
PA66
Want to keep this datasheet? Save it now in your required format

Description

Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including most flame retardant grades, offer the ability to be coloured. The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.14 g/cm³

Show Material materials with Density of 1.14 g/cm³

ISO 1183

Water absorption

23.0 °C

8.5 %

Show Material materials with Water absorption of 8.5 %

Sim. to ISO 62 | 80mil

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3 GPa

Show Material materials with Elastic modulus of 3 GPa

ISO 527-1/-2

Elongation

23.0 °C

32 %

Show Material materials with Elongation of 32 %

ISO 527-1/-2 | 50mm/min

Elongation at yield

23.0 °C

4.5 %

Show Material materials with Elongation at yield of 4.5 %

ISO 527-1/-2

Flexural modulus

23.0 °C

2.8 GPa

Show Material materials with Flexural modulus of 2.8 GPa

ISO 178

Flexural strength

23.0 °C

115 MPa

Show Material materials with Flexural strength of 115 MPa

ISO 178

Hardness, Rockwell R

23.0 °C

121 [-]

Show Material materials with Hardness, Rockwell R of 121 [-]

ISO 2039-2

Impact strength, Charpy notched

23.0 °C

5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eA

Impact strength, Izod unnotched

-40.0 °C

4 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 4 kJ/m²

ISO 180/1A

23.0 °C

5 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 5 kJ/m²

ISO 180/1A

Poisson's ratio

23.0 °C

0.37 [-]

Show Material materials with Poisson's ratio of 0.37 [-]

Yield strength

23.0 °C

84 MPa

Show Material materials with Yield strength of 84 MPa

ISO 527-1/-2

Impact strength, Charpy unnotched

No Break @ 23°C, ISO 179/1eU

Thermal

PropertyTemperatureValueComment

Heat deflection temperature, 0.45 MPa

200 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 200 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

70 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 70 °C

ISO 75-1/-2

Melting point

263 °C

Show Material materials with Melting point of 263 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B | 240mil

Relative temperature index, mechanical impact

75 °C

Show Material materials with Relative temperature index, mechanical impact of 75 °C

UL 746B | 240mil

Relative temperature index, mechanical strength

85 °C

Show Material materials with Relative temperature index, mechanical strength of 85 °C

UL 746B | 240mil

Specific heat capacity

23.0 °C

2790 J/(kg·K)

Show Material materials with Specific heat capacity of 2790 J/(kg·K)

of melt

Vicat softening temperature

257 °C

Show Material materials with Vicat softening temperature of 257 °C

ISO 306 | 90°F/h, 11 lbf

Flammability

Burning Behav. at 60mil nom. thickn.: V-2 class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: V-2 class, Thickness tested: 0.71 mm, UL recognition: yes -, Oxygen index: 24 %, Glow Wire Flammability Index, 15mil: 900 °C, Glow Wire Flammability Index, 30mil: 900 °C, Glow Wire Flammability Index, 60mil: 960 °C, Glow Wire Flammability Index, 80mil: 960 °C, Glow Wire Flammability Index, 120mil: 960 °C, Glow Wire Ignition Temperature, 40mil: 825 °C, Glow Wire Ignition Temperature, 80mil: 750 °C, Glow Wire Ignition Temperature, 120mil: 775 °C, Glow Wire Temperature, No Flame, 40mil: 750 °C, Glow Wire Temperature, No Flame, 80mil: 725 °C, FMVSS Class: SE -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Material materials with Comparative tracking index of 600 V

IEC 60112

Dielectric strength

23.0 °C

27 kV/mm

Show Material materials with Dielectric strength of 27 kV/mm

IEC 60243-1

Dissipation factor, 100Hz

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor, 100Hz of 0.01 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor, 1MHz of 0.01 [-]

IEC 62631-2-1

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Material materials with Volume resistivity of 1.00E+15 Ω·cm

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1.5 %

Show Material materials with Shrinkage of 1.5 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1.5 %

Show Material materials with Shrinkage, transverse of 1.5 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 70°C, Min. mold temperature: 50°C, Max. mold temperature: 90°C, Hold pressure range: 50-100MPa, Hold pressure time: 4s/mm, Ejection temperature: 190°C