Zytel® LC6210 BK010

Alternative and trade names
PA612-HI
Want to keep this datasheet? Save it now in your required format

Description

DuPont™ Zytel® LCPA long chain polyamide resins provide an innovative and growing portfolio of flexible polymers with excellent thermal, chemical, and hydrolysis resistance. The diverse selection of Zytel® LCPA grades is targeted for a range of performance characteristics, balancing temperature resistance, flexibility and low permeation.Zytel® LC6210 BK010 is a toughened polyamide 612 resin for extrusion applications.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.01 g/cm³

Show Material materials with Density of 1.01 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.1 GPa

Show Material materials with Elastic modulus of 1.1 GPa

ISO 527-1/-2

Elongation

23.0 °C

100 %

Show Material materials with Elongation of 100 %

ISO 527-1/-2 | 50mm/min

Elongation at yield

23.0 °C

12 %

Show Material materials with Elongation at yield of 12 %

ISO 527-1/-2

Impact strength, Charpy notched

-6.0 °C

13 kJ/m²

Show Material materials with Impact strength, Charpy notched of 13 kJ/m²

ISO 179/1eA

23.0 °C

35 kJ/m²

Show Material materials with Impact strength, Charpy notched of 35 kJ/m²

ISO 179/1eA

Poisson's ratio

23.0 °C

0.45 [-]

Show Material materials with Poisson's ratio of 0.45 [-]

Yield strength

23.0 °C

33 MPa

Show Material materials with Yield strength of 33 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.5E-4 1/K

Show Material materials with Coefficient of thermal expansion of 2.5E-4 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

1.2E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.2E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

83 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 83 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

47 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 47 °C

ISO 75-1/-2

Melting point

216 °C

Show Material materials with Melting point of 216 °C

ISO 11357-1/-3 | 18°F/min

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Technological properties

Property