Zytel® RS LC3160 NC010

Want to keep this datasheet? Save it now in your required format

Description

Zytel® RS LC3160 NC010 isan unreinforced, medium viscosity grade, biobased polyamide 610 developed for extrusion applications.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.07 g/cm³

Show Material materials with Density of 1.07 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.14 GPa

Show Material materials with Elastic modulus of 2.14 GPa

ISO 527-1/-2

Elongation

23.0 °C

500 %

Show Material materials with Elongation of 500 %

min. | ISO 527-1/-2

Elongation at yield

23.0 °C

3.5 %

Show Material materials with Elongation at yield of 3.5 %

ISO 527-1/-2

Impact strength, Charpy notched

23.0 °C

6 kJ/m²

Show Material materials with Impact strength, Charpy notched of 6 kJ/m²

ISO 179/1eA

Poisson's ratio

23.0 °C

0.39 [-]

Show Material materials with Poisson's ratio of 0.39 [-]

Yield strength

23.0 °C

58 MPa

Show Material materials with Yield strength of 58 MPa

ISO 527-1/-2

Thermal

PropertyValue

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Technological properties

Property