Poly(ether sulfone), 30% Glass Fiber Reinforced (PES-GF30)

Alternative and trade names
PES, Victrex 430P
Want to keep this datasheet? Save it now in your required format

Description

Poly(ether sulfone) is a high performance thermoplastic of relatively low flammability. It offers amorphous, high-creep resistance and stable electrical properties over wide temperature and frequency ranges. Poly(ether sulfone) is transparent with good thermal and hydrolytic resistance.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.6 g/cm³

Show Material materials with Density of 1.6 g/cm³

Water absorption

23.0 °C

0.43 %

Show Material materials with Water absorption of 0.43 %

24h

Mechanical

PropertyTemperatureValue

Flexural modulus

23.0 °C

6.99 GPa

Show Material materials with Flexural modulus of 6.99 GPa

Flexural strength

23.0 °C

210 MPa

Show Material materials with Flexural strength of 210 MPa

Hardness, Shore D

23.0 °C

86 [-]

Show Material materials with Hardness, Shore D of 86 [-]

Impact strength, Izod notched, ASTM

23.0 °C

296 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 296 J/m

Impact strength, Izod unnotched, ASTM

23.0 °C

1082 J/m

Show Material materials with Impact strength, Izod unnotched, ASTM of 1082 J/m

Tensile strength

23.0 °C

146.9 MPa

Show Material materials with Tensile strength of 146.9 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.3E-5 1/K

Glass transition temperature

224.85 °C

Show Material materials with Glass transition temperature of 224.85 °C

Forced oscillation dynamic-mechanical analysis

Heat deflection temperature, 1.80 MPa

202.85 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 202.85 °C

ASTM D648

Max service temperature

217.85 °C

Show Material materials with Max service temperature of 217.85 °C

Thermal conductivity

23.0 °C

0.18 W/(m·K)

Show Material materials with Thermal conductivity of 0.18 W/(m·K)

Electrical

PropertyTemperatureValue

Dielectric constant

23.0 °C

3.5 [-]

Show Material materials with Dielectric constant of 3.5 [-]

Electrical resistivity

23.0 °C

1.00E+15 Ω·m

Show Material materials with Electrical resistivity of 1.00E+15 Ω·m

Optical

PropertyValue

Refractive index

1.55 [-]

Show Material materials with Refractive index of 1.55 [-]

Acoustical

PropertyTemperatureValue

Sound speed, longitudinal

23.0 °C

2260 m/s

Show Material materials with Sound speed, longitudinal of 2260 m/s

Technological properties

Property
Application areas

Medical and household appliances that are sterilizable by hot air and steam such as corrosion-resistant piping. Also used in electric and electronic applications such as television components. Used as membranes for reverse gas streams and gas separation.

Fillers

30% Glass Fiber