Description

Poly(N-vinyl carbazole) offers a high heat distortion temperature, outstanding dielectric properties for electrical uses and a high refractive index for optical uses.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Material materials with Density of 1.19 g/cm³

Water absorption

23.0 °C

0.1 %

Show Material materials with Water absorption of 0.1 %

max.

Mechanical

PropertyTemperatureValue

Compressive strength

23.0 °C

30 - 35 MPa

Show Material materials with Compressive strength of 30 - 35 MPa

Elastic modulus

23.0 °C

2.5 - 4.2 GPa

Show Material materials with Elastic modulus of 2.5 - 4.2 GPa

Elongation

23.0 °C

1 %

Show Material materials with Elongation of 1 %

Flexural strength

23.0 °C

35 - 55 MPa

Show Material materials with Flexural strength of 35 - 55 MPa

Hardness, Ball Indentation

23.0 °C

100 MPa

Show Material materials with Hardness, Ball Indentation of 100 MPa

Shear strength

23.0 °C

20 - 30 MPa

Show Material materials with Shear strength of 20 - 30 MPa

Tensile strength

23.0 °C

140 MPa

Show Material materials with Tensile strength of 140 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5E-5 1/K

Show Material materials with Coefficient of thermal expansion of 5E-5 1/K

for 23 to 100°C

Thermal conductivity

20.0 °C

1.26E-3 W/(m·K)

Show Material materials with Thermal conductivity of 1.26E-3 W/(m·K)

170.0 °C

1.68E-3 W/(m·K)

Show Material materials with Thermal conductivity of 1.68E-3 W/(m·K)

Vicat softening temperature

194.85 °C

Show Material materials with Vicat softening temperature of 194.85 °C

Electrical

PropertyTemperatureValueComment

Dielectric constant, 100Hz

23.0 °C

3 [-]

Show Material materials with Dielectric constant, 100Hz of 3 [-]

Dielectric strength

23.0 °C

86 - 110 kV/mm

Show Material materials with Dielectric strength of 86 - 110 kV/mm

Electrical resistivity

23.0 °C

1.00E+14 - 1.00E+15 Ω·m

Show Material materials with Electrical resistivity of 1.00E+14 - 1.00E+15 Ω·m

DIN 57303

Optical

PropertyValue

Refractive index

1.69 [-]

Show Material materials with Refractive index of 1.69 [-]

Technological properties

Property
Application areas

Photoconductor