APTIV® 1000 Series Film 25µm

Alternative and trade names
APTIV® 1000 Series Film 25µm
Want to keep this datasheet? Save it now in your required format

Description

APTIV® 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 1000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Thickness

0.03 mm

Show Material materials with Thickness of 0.03 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.6 GPa

Show Material materials with Elastic modulus of 2.6 GPa

ISO 527

Elastic modulus, transverse

23.0 °C

2.8 GPa

Show Material materials with Elastic modulus, transverse of 2.8 GPa

ISO 527

Elongation

23.0 °C

150 %

Show Material materials with Elongation of 150 %

ISO 527

Elongation, transverse

23.0 °C

150 %

Show Material materials with Elongation, transverse of 150 %

ISO 527

Tensile strength

23.0 °C

140 MPa

Show Material materials with Tensile strength of 140 MPa

ISO 527

Tensile strength, transverse

23.0 °C

120 MPa

Show Material materials with Tensile strength, transverse of 120 MPa

ISO 527

Thermal

PropertyValue

Glass transition temperature

146 °C

Show Material materials with Glass transition temperature of 146 °C

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

6.75 kV

Show Material materials with Breakdown voltage of 6.75 kV

ASTM D149 (6.25mm electrode)

Dielectric strength

23.0 °C

270 kV/mm

Show Material materials with Dielectric strength of 270 kV/mm

ASTM D149 (6.25mm electrode)

Technological properties

Property
Application areas

Electrical insulation, pressure sensitive tapes, printed circuit substrates, high temperature labels, washers in high speed motors, washers in mobile phone hinges, flexible surface heaters, aerospace insulation, pressure sensor membranes, acoustic speaker diaphragms, capacitors, composites, proven temperature resistance to use of lead free solders

Certifications

APTIV® film is FDA and EU approved for food contact and is RoHS and 3A Sanitary Standards compliant.

Other

The key features are: High heat resistance, excellent tribological properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent barrier properties, excellent acoustic properties, high purity, lightweight, recyclable, easy to process

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.