APTIV® 2000 Series Film 25µm

Alternative and trade names
APTIV® 2000 Series Film 25µm
Want to keep this datasheet? Save it now in your required format

Description

APTIV® 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 2000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.


Please note - APTIV 2000 will crystallise if taken above the Tg [143°C (289°F)] in either secondary processes or end use application. The crystallisation is not reversible back to the amorphous phase without re-melting the material. Consideration of the temperature range during processing and end use application needs to be included if selecting APTIV 2000.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Thickness

0.03 mm

Show Material materials with Thickness of 0.03 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.8 GPa

Show Material materials with Elastic modulus of 1.8 GPa

ISO 527

Elastic modulus, transverse

23.0 °C

1.8 GPa

Show Material materials with Elastic modulus, transverse of 1.8 GPa

ISO 527

Elongation

23.0 °C

200 %

Show Material materials with Elongation of 200 %

ISO 527

Elongation, transverse

23.0 °C

200 %

Show Material materials with Elongation, transverse of 200 %

ISO 527

Tensile strength

23.0 °C

130 MPa

Show Material materials with Tensile strength of 130 MPa

ISO 527

Tensile strength, transverse

23.0 °C

130 MPa

Show Material materials with Tensile strength, transverse of 130 MPa

ISO 527

Thermal

PropertyValue

Glass transition temperature

143 °C

Show Material materials with Glass transition temperature of 143 °C

Electrical

PropertyTemperatureValueComment

Breakdown voltage

23.0 °C

6.75 kV

Show Material materials with Breakdown voltage of 6.75 kV

ASTM D149 (6.25mm electrode)

Dielectric strength

23.0 °C

270 kV/mm

Show Material materials with Dielectric strength of 270 kV/mm

ASTM D149 (6.25mm electrode)

Technological properties

Property
Application areas

Aerospace insulation, electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts, composites

Certifications

APTIV 2000 film is approved for Food Contact Use: APTIV 2000 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2000 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2000 film is fully compliant with the 3-A Sanitary Standards. APTIV film 2000 complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2000 film is inherently halogen-free in accordance with IEC61249-2-21.

Other

The key features are: High heat resistance, excellent Flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process.

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. APTIV 2000 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms: Surface treatment, adhesion, coatings, slitting, die cutting and stamping, thermal lamination, heat welding and heat sealing, metallisation, laser marking and machining, thermoforming, printing